MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Kraton® D4153 E (O/E SBS) Linear Block Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D4153 E is an oil-extended linear block copolymer based on styrene and butadiene with bound styrene in the neat polymer of 35% mass. It contains 40 phr paraffinic oil which is classified as not hazardous. Information on the CAS and EINECS registry numbers of the paraffinic oil used for this grade is available on request. The product is supplied from Europe in the physical form identified:
Kraton D4153 ES - supplied as porous pellets dusted with an amorphous silica
Kraton D4153 ESM - supplied as powder dusted with an amorphous silica

Region: North America, Europe, Asia Pacific, Japan, and South America

Uses: Kraton D4153 E is used in formulating compounds for footwear, technical and general purpose applications. It can also be used in formulating adhesives, sealants and coatings and as a modifier of bitumen.

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; and Roads and Roofing

Information provided by Kraton®

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Bulk Density, ASTM D 1895 method B
  • Volatiles, KM 04
  • Melt Flow, ISO 1133
  • Ash, ISO 247, ES
  • Ash, ISO 247, ESM
  • Hardness, Shore A, ISO 868, Measured on injection molded slabs
  • Tensile Strength, ASTM D412, Measured on injection molded slabs
  • Elongation at Break, ISO 37, Measured on injection molded slabs
  • 300% Modulus, ISO 37, Measured on injection molded slab
  • Abrasion, DIN 53516, [cubic mm], Measured on injection molded slabs
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.