MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Morgan Advanced Ceramics Thermo-Bloc Modules Ceramic Fiber Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Thermo-Bloc modules are manufactured from two sections of Pyrolog™ slabs in edge-grain orientation. These are held in position by a 6 faces polythene plastic film that ensures also the mechanical protection of the fibre and the protection of the installers from dust exposure. Thermo-Bloc Modules are installed with a pre-studded, external, side-fax yoke. This system permits the introduction of backing blankets and of anti-corrosion treatments of the casing, following the design of the customers or with Morgan Thermal Ceramics anchor designs. For special roof applications, the two sections of Pyrolog™ slabs can be held in position by two additional stainless steel tubes mounted transversely through the modules and remote from the hot face. The side fixed yokes fit in these tubes. The design of linings made with Thermo-Bloc Modules can be completed with the use of special shapes obtained from Pyrolog slabs to line corners, noses and other particular zones.

Typical Applications:

  • Thermo-Blocs have a multitude of uses in heat containment applications in all industry groups, a selection of which are as follows.
  • Utilities Thermal Oxidisers, Waste Heat Recovery Units, Combusion Chambers, Boiler Ductwork, Process Heaters, Crude Heaters
  • Iron and Steel Soaking Pit Covers, Multi and Single Stack Coil Annealing Furnaces, Continuous Annealing and Coating Furnaces, Rotary Hearth Furnaces, Car Bottom Furnaces, Roller Furnaces, Offtakes and Ductwork
  • Aluminium Soaking Pits and Covers, Homogenising Furnaces, Ductwork, Transfer Ladies Lids and Launders Lids

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors:
Available Properties
  • Density
  • Specific Heat Capacity
  • Thermal Conductivity, at 192 kg/m3
  • Thermal Conductivity, at 160 kg/m3
  • Thermal Conductivity, at 192 kg/m3
  • Thermal Conductivity, at 160 kg/m3
  • Thermal Conductivity, at 192 kg/m3
  • Thermal Conductivity, at 160 kg/m3
  • Thermal Conductivity, at 192 kg/m3
  • Thermal Conductivity, at 160 kg/m3
  • Shrinkage, isothermal
  • Loss on Ignition(%)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.