MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Eastman D4036-F Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and general-purpose packaging

List of Applications:

  • Films
  • Packaging

D4036-F meets the requirements of FDA regulations at 21 CFR 177.1520(c)(2.2) and may be used as a component of packages used for holding food during cooking. However, the polymer thickness in the form in which it contacts food shall not exceed 0.005 inches and contact is limited to non-alcoholic food because of a regulatory limitation for an adjuvant substance in this formulation.

Information supplied by the manufacturer.

Information from manufacturer data sheet.

Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.

Key Words: Good balance of properties
Vendors:
Available Properties
  • Density, ASTM D4883
  • Moisture Vapor Transmission, ASTM F372
  • Oxygen Transmission, ASTM D1434
  • Thickness
  • Melt Flow, ASTM D1238
  • Film Tensile Strength at Yield, MD, ASTM D882
  • Film Tensile Strength at Yield, TD, ASTM D882
  • Film Elongation at Break, MD, ASTM D882
  • Film Elongation at Break, TD, ASTM D882
  • Secant Modulus, MD, 1% Secant; ASTM D882
  • Secant Modulus, TD, 1% Secant; ASTM D882
  • Coefficient of Friction, ASTM D1894
  • Elmendorf Tear Strength MD
  • Elmendorf Tear Strength TD
  • Elmendorf Tear Strength, MD, ASTM D1922
  • Elmendorf Tear Strength, TD, ASTM D1922
  • Dart Drop, ASTM D1709A
  • Film Tensile Strength at Break, MD, ASTM D882
  • Film Tensile Strength at Break, TD, ASTM D882
  • Vicat Softening Point, ASTM D1525
  • Haze, ASTM D1003
  • Gloss, at 45°; ASTM D2457
  • Transmission, Visible, ASTM D1746
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.