MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Solvay Evolite™ F1050 Thermoplastic PVDF/Carbon Fiber Composite
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), with Carbon Fiber

Material Notes: Evolite™ F1050 is a high performance thermoplastic composite material specially designed for the O&G industry. EvoliteTM F1050 is a unidirectional tape combining the recognized excellent chemical and temperature resistance of Solef® PVDF with the inherent high strength performance of carbon fiber.

Features:

  • Semi crystalline PVDF thermoplastic matrix
  • Compatibility within PVDF Solef® 60512 and other Solef® grades
  • Fully impregnated unidirectional tape
  • Maximum Service Temperature of 130°C
  • Customised Fibre/Matrix translation for maximum performance
  • Ideal processing, mechanical and chemical resistance for applications in Oil & Gas
  • Recyclable
  • 5 year storage at ambient conditions

    Information provided by Solvay.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Thickness, Tape
  • Tensile Strength, EN 2597:1998, 90° tape property
  • Tensile Strength, ASTM D3039M, 0° tape property
  • Tensile Strength, ASTM D3039, 0° tape property after autoclave consolidation
  • Tensile Modulus, ASTM D3039M, 0° tape property
  • Tensile Modulus, ASTM D3039, 0° tape property after autoclave consolidation
  • Compressive Strength, ASTM D6641, 0° tape property after autoclave consolidation
  • Shear Modulus, ASTM D3518 , IPSS, 45° tape property after autoclave consolidation
  • Shear Strength, ASTM D3518 , IPSS, 45° tape property after autoclave consolidation
  • Shear Strength, ASTM D2344, ILSS, 0° tape property after autoclave consolidation
  • Melting Point, ASTM D3418
  • Glass Transition Temp, Tg, ASTM D4065
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.