MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP21TPFL-1 Two Component Low Viscosity Epoxy Polysulfide Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Polysulfide Sealant/Adhesive

Material Notes: Key Features:
  • High flexibility
  • First rate electrical insulator
  • Good chemical resistance
  • Cures at room temperature
Product Description: Master Bond EP21TPFL-1 is a two component, low viscosity epoxy polysulfide system, which upon curing, offers a highly special combination of flexibility and chemical resistance. EP21TPFL-1 has excellent resistance to a wide array of chemicals including water, gasoline, fuels, oils, hydrocarbons and hydraulic fluids. It has been formulated to cure readily at ambient temperatures. Unlike most two part epoxies, heat curing is not recommended. This system has a non-critical mix ratio of one to two, by weight or volume. EP21TPFL-1 has good physical strength and superior electrical insulation properties. This allows the system to be utilized in situations involving rigorous thermal cycling as well as thermal and mechanical shocks. It has very good adhesion to metals, ceramics, glass, and many rubbers and plastics. Since it is a first class insulator, with low viscosity as well as low exotherm, it is serviceable as a potting and encapsulation system. The service temperature range is -60°F to +250°F. The color of Part A is clear while Part B is brown. Polysulfide systems have been traditionally used for many years as fuel tank sealants, as well as for electrical connectors exposed to fuels, oils and lubricants, for many years. EP21TPFL-1 can also be used in aerospace, electronic and specialty OEM, among other applications, where this highly unusual combination of superb flexibility along with superior chemical resistance is desirable.

Product Advantages:

  • Convenient mixing: forgiving one to two mix ratio by weight or volume
  • Low viscosity enhances ease of application, compound flows evenly and smoothly; ideal for potting
  • Cures at ambient temperatures
  • 100% reactive — no volatiles emitted during curing
  • Outstanding flexibility with superior resistance to thermal cycling
  • Polysulfide type chemical resistance profile

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, mixed
  • Viscosity, Part A
  • Hardness, Shore A
  • Tensile Strength
  • Elongation at Break
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.