MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chesterton 740 Heavy Duty Rust Guard
Categories: Fluid

Material Notes: Description: Chesterton® 740 Heavy Duty Rust Guard is a premium quality corrosion preventative coating designed with user ease of application in mind. It is the perfect coating for those areas of the plant constantly exposed to humidity and corrosive fumes. It protects iron, steel, aluminum and other metals in industrial, automotive and marine applications indoors and outdoors (sheltered) for up to 2 years. Chesterton 740 Heavy Duty Rust Guard is easy to apply, requiring minimum surface preparation. It can be applied by dipping, brushing or with convenient aerosol spray. After thorough removal of loose scale, 740 Heavy Duty Rust Guard can be applied to rusted surface to prevent further corrosion. It can also be applied to rusted surface to prevent further corrosion. It can also be applied directly over Chesterton® 763 Rust Transformer® without a water rinse for an excellent 1-2 barrier system. Chesterton 740 Heavy Duty Rust Guard is long lasting durable. The tough coat deposited with even a single application approaches the performance of many paints.

Features:

  • Excellent resistance to acid, alkali and salt air fumes
  • Dry wax film
  • Self-healing if scratched
  • Easy to apply – Easy to remove
  • Does not flake or peel
  • Provides up to two years corrosion protection under sheltered outdoor conditions
  • Withstands up to 2000 hours in accelerated corrosion test (ASTM B117)
  • Conforms to United States Military Specifications MIL-C-16173D, Grade 1 and 4

Applications: Protects iron and steel from rusting indoors or outdoors for up to two years. Gives long lasting protection for metal, tools, fixtures, parts-in-process, equipment tanks, roofs, structures, machinery tubing, castings, rod, bar and sheet stock. Keeps rust from forming on jigs, fixtures, sheet stock, stampings, parts in storage. Spray on pumps, fittings, valves, and hinges; and area subject to humidity and water exposure. Recommended for lay-up protection on chrome and brass fixtures, engine blocks. Protects automobiles and equipment during overseas shipment. Protects construction equipment, pipe, or machinery stored out of doors against corrosion.

Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • Solids Content, bulk, by volume
  • Solids Content, bulk, by weight
  • Thickness, Dry Recommended Film
  • Thickness, Wet Recommended Film
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point
  • Flash Point, ASTM D56, Closed Cup
  • Ignition Temperature, ASTM D2155, Autoignition
  • Processing Temperature, Application Temperature
  • Processing Temperature, Application Temperature
  • Dry Time, Complete
  • Tack-Free Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.