MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
MOL Group TIPELIN BB 620-17 HDPE, Blow molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Description: TIPELIN BB 620-17 is a high density polyethylene copolymer (with hexen-1 as comonomer) grade for blow molding of products which require high rigidity. The grade contains antioxidant.

Applications: TIPELIN BB 620-17 is recommended for shrink films, multi-layer films and blend component for LDPE for applications where high stiffness is required. It can be used in the middle layer in a coex structure or blended with LDPE and LLDPE to increase stiffness and film strength. The product is also suitable for blow molding of small size bottles. Furthermore, it is suitable for corrugated pipes too.

(1) Average mechanical property values of several measurements carried out on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291). (2) Average mechanical property values of several measurements on film (MD = machine direction, TD = trans direction) thickness of 0.025 mm, blow up ratio 4:1.

Information provided by Molgroup Chemicals

Vendors:
Available Properties
  • Density, ISO 1183-1, 1
  • ESCR 100% IgepalĀ®, ASTM D 1693, 1, CO-630
  • Oxidative Induction Time (OIT), EN 728
  • Melt Flow, ISO 1133-1
  • Melt Flow, ISO 1133-1
  • Melt Flow, ISO 1133-1
  • Storage Temperature
  • Hardness, Shore D, ISO 868, 1
  • Film Tensile Strength at Yield, MD, ISO 527-3, 2
  • Film Tensile Strength at Yield, TD, ISO 527-3, 2
  • Tensile Strength, Yield, ISO 527-3, 1
  • Film Elongation at Break, MD, ISO 527-3, 2
  • Film Elongation at Break, TD, ISO 527-3, 2
  • Elongation at Break, ISO 527-3, 1
  • Elongation at Yield, ISO 527-3, 1
  • Flexural Modulus, ISO 178, 1
  • Izod Impact, Notched (ISO), ISO 180/A, 1
  • Impact, ASTM D 3420, 2, Spencer
  • Elmendorf Tear Strength MD, ISO 6383-2, 2
  • Elmendorf Tear Strength TD, ISO 6383-2, 2
  • Dart Drop Test, ISO 7765-1 method A, 2, F50
  • Film Tensile Strength at Break, MD, ISO 527-3, 2
  • Film Tensile Strength at Break, TD, ISO 527-3, 2
  • Vicat Softening Point, ISO 306/A 120, 1
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.