Kaowool Flexi-Felt is manufactured from high purity refractory fibres and designed for high temperature insulation up to 1260°C with a minimum addition of carefully selected bonds. Kaowool Flexi-Felt exhibits excellent strength, flexibility and is pleasant to handle, cuts cleanly and is ideally suited for the manufacture of the most intricate die-cut shapes and gaskets, even in thin section, and is available in roll form which permits maximum material utilization offering improved flexibility to the die-cutter. Other beneficial properties include low thermal conductivity, low thermal mass and exceptionally high thermal shock resistance. Applications: - Expansion joints for refractory bricks
- High temperature gaskets
- Investment casting mould wrapping
- Back-up lining
- Combustion chamber lining
- Thermal shields
Information provided by Morgan Advanced Materials |