MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Akrochem DF55 5,000 Silicone fluid
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: The DF55 series of silicone fluids are 100% crystal clear dimethylpolysiloxane polymers with a viscosity range of 50 - 60,000 centistokes. Their outstanding characteristics are that of inertness, heat stability, oxidation stability, good electrical properties, low pour point and nontoxicity. Some of the general applications are as release and slip agents, additives in rubber and plastics for special surface properties and water repellent treatments.

Applications: Silicone fluids are preferred over silicone emulsions where mold build up cannot be tolerated. Silicone fluids are normally cut for spray applications with non-polar solvents. The advantages of this are: less mold build up from emulsifiers used in silicone emulsions, provides rapid flash off on hot surfaces and the silicone can be used on molds where the flash temperature of water is higher than that of the mold surface. Silicone Fluids are suggested as good general purpose release agents for most tire and mechanical goods operations such as: tire molds and curing bags, shock mounts, fan belts, "O" rings, floor mats, hose, toys, shoe heels and soles, floor tile, rubber runners, bath mats, etc. Some wire and cable applications include easy stripping of insulation from wire, braiding of silver-plated or tin-coated wire and lead sheath removal.

Information provided by Akrochem Corporation

Vendors:
Available Properties
  • Specific Gravity
  • Volatiles
  • Viscosity Measure
  • Flash Point, closed cup
  • Refractive Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.