MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Hexcel® HexBond™ ST1480.03 NW 146g/m2 Epoxy Film Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: HexBond™ ST1480 is a modified epoxy film adhesive. This 180°C/356°F cure film adhesive is specially designed for bonding metal-to-metal and composite-to-composite structures. Its formulation, based on epoxy resin, provides high peel strength and toughness with high sheer strength.

Features:

  • Excellent metal-to-metal peel strength and composite-to-composite bonding
  • 180°C/356°F cure
  • Service temperature from -55°C to 150°C (-67°F to 302°F)
  • Excellent moisture resistance in high humidity environments
  • Available in a wide range of film thicknesses
Applications:
  • Metal-to-metal bonding
  • Sandwich construction
  • Composite-to-composite bonding
Cure 1: 90 min at 180°C
Cure 2: 4h at 150°C

Information provided by Hexcel Corporation.

Vendors:
Available Properties
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal, 2000 hours 70°C / 158°F 85% RH, Cure 2
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal, 2000 hours 70°C / 158°F 85% RH, Cure 1
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, Cure 1
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, Cure 2
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal, 2000 hours 70°C / 158°F 85% RH, Cure 2
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, 2000 hours 70°C in hydraulic fluid
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal, 2000 hours 70°C / 158°F 85% RH, Cure 1
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, Cure 2
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, Cure 1
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, 2000 hours 70°C in hydraulic fluid
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, 2000 hours 50°C in hydraulic fluid/water mixture
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, Cure 1
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, Cure 2
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, 2000 hours 50°C in hydraulic fluid/water mixture
  • Adhesive Bond Strength, AITM 1-0019, Single Lap Shear Strength Composite/Composite, Cure 1
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, 2000 hours 70°C / 158°F 85% RH, Cure 1
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, Cure 2
  • Adhesive Bond Strength, AITM 1-0019, Single Lap Shear Strength Composite/Composite, 2000 hours 70°C / 158°F, Cure 1
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, 24 hours 23°C in solvent
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, 2000 hours 70°C / 158°F 85% RH, Cure 2
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, Cure 1
  • Adhesive Bond Strength, AITM 1-0019, Single Lap Shear Strength Composite/Composite, 2000 hours 70°C / 158°F, Cure 2
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, 24 hours 23°C in solvent
  • Adhesive Bond Strength, AITM 1-0019, Single Lap Shear Strength Composite/Composite, 2000 hours 70°C / 158°F 85% RH, Cure 2
  • Adhesive Bond Strength, EN 2243-1, Single Lap Shear Strength Metal/Metal, Cure 1
  • Adhesive Bond Strength, AITM 1-0019, Single Lap Shear Strength Composite/Composite, 2000 hours 70°C / 158°F, Cure 1
  • Adhesive Bond Strength, AITM 1-0019, Single Lap Shear Strength Composite/Composite, Cure 1
  • Adhesive Bond Strength, AITM 1-0019, Single Lap Shear Strength Composite/Composite, 2000 hours 70°C / 158°F 85% RH, Cure 1
  • Adhesive Bond Strength, AITM 1-0019, Single Lap Shear Strength Composite/Composite, 2000 hours 70°C / 158°F, Cure 2
  • Adhesive Bond Strength, AITM 1-0019, Single Lap Shear Strength Composite/Composite, Cure 1
  • Glass Transition Temp, Tg, 4h at 150°C, 2000 hours 70°C / 158°F
  • Glass Transition Temp, Tg, 90 min at 180°C, 2000 hours 70°C / 158°F 85% RH
  • Glass Transition Temp, Tg, 4h at 150°C
  • Glass Transition Temp, Tg, 90 min at 180°C
  • Cure Time
  • Cure Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.