MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Master Bond EP110F8-3 Two component, high performance epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Key Features:
  • Toughened system
  • Low viscosity and long working life
  • Outstanding electrical insulation properties
  • Very resistant to thermal cycling and shock
Master Bond EP110F8-3 is a two component high performance epoxy resin system with a long pot life (at least 2-3 days at room temperature). It is used primarily for potting, sealing, encapsulating and casting. This low viscosity system has a convenient and very forgiving one to two mix ratio by weight. It requires an elevated temperature cure at 250-300°F. A typical cure schedule would be 4-6 hours at 250-300°F. For optimum properties, a post cure of 3-5 hours at 350°F is recommended. Even without the optional post cure, EP110F8-3 will perform very well. EP110F8-3 has no solvents or diluents and has low shrinkage upon cure. It adheres well to a wide variety of substrates, including metals, composites, glass and many plastics. It has superior electrical insulation properties. Its physical strength properties of low tensile strength, lower modulus and relatively higher elongation, translates into a special capability to resist severe thermal cycling and shock. It has good resistance to water, oils and fuels. The color of Part A is clear while the color of Part B is amber. The service temperature range is -100°F to +300°F. It can be used in applications where very high performance electrical insulation properties and resistance to rigorous thermal cycling is needed.

Product Advantages:

  • Low viscosity liquid; flows easily
  • Long working life at room temperature
  • Outstanding thermal shock resistance
  • Very high elongation
  • Unsurpassed electrical insulation properties

Information provided by Masterbond.

Vendors:
Available Properties
  • Viscosity, mixed
  • Viscosity, Part B
  • Viscosity, Part A
  • Hardness, Shore A
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Constant
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Optional post cure
  • Cure Time
  • Shelf Life, In original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.