MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Pressure Seal 9765 Fluorinated Hydrocarbon
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 9765 is a 70 durometer cream colored Fluoroelastomer, it is formulated with FDA approved materials. It exhibits good resistance to petroleum based oils and aromatic fuels. This compound is also suitable for milk and edible oils.

This compound will meet or exceed the specifications listed and has the following physical properties: 3-A Sanitary 18-03 Class I, II, III, & IV
CFR 21 177.2600

Information provided by Pressure Seals Inc.

Vendors:
Available Properties
  • Specific Gravity
  • Hardness, Shore A
  • Hardness, Shore A, Stauffer Blend 7700
  • Hardness, Shore A, Heat Aged
  • Hardness, Shore A, Heat Aged
  • Hardness, Shore A, Service Fluid 101
  • Hardness, Shore A, Distilled water aged
  • Hardness, Shore A, ASTM Reference Fuel C
  • Hardness, Shore A, ASTM Oil #1 (IRM 901)
  • Hardness, Shore A, ASTM Oil #3 (IRM 903)
  • Tensile Strength
  • Tensile Strength, Stauffer Blend 7700
  • Tensile Strength, Service Fluid 101
  • Tensile Strength, ASTM Reference Fuel C
  • Tensile Strength, Heat Aged
  • Tensile Strength, ASTM Oil #3 (IRM 903)
  • Tensile Strength, ASTM Oil #1 (IRM 901)
  • Tensile Strength, Heat Aged
  • Elongation, Ultimate
  • Elongation, Ultimate, Heat Aged
  • Elongation, Ultimate, Stauffer Blend 7700
  • Elongation, Ultimate, Service Fluid 101
  • Elongation, Ultimate, ASTM Reference Fuel C
  • Elongation, Ultimate, ASTM Oil #1 (IRM 901)
  • Elongation, Ultimate, ASTM Oil #3 (IRM 903)
  • Elongation, Ultimate, Heat Aged
  • 100% Modulus
  • Tear Strength, Die C
  • Tear Strength, Die B
  • Compression Set, Plied
  • Compression Set, Plied
  • Compression Set, Plied
  • Brittleness Temperature
  • Shrinkage, Volume, ASTM Oil #1
  • Shrinkage, Volume, ASTM Oil #3
  • Shrinkage, Volume, Distilled water aged
  • Shrinkage, Volume, ASTM Reference Fuel C
  • Shrinkage, Volume, Service Fluid 100
  • Shrinkage, Volume, Stauffer Blend 7700
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.