MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Go Yen Chemical GOYENCHEM-PTFE Anti-dripping Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GOYENCHEM-PTFE, anti-dropping flame retardant, is provided by GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC GROUP), that work with GY-FR-OP series. When adding into Thermoplastic plastic, due to heat effect, it will generate GOYENCHEM-PTFE microball, which more than 0.18µm, and form cross-link network in the process of pressing and cutting. When burned, this network will contract, then consequently, trap the melted polymer, insulate oxygen, accelerate the carbonization of polymer, and therefore, makes the polymer flame-retarded. GY-PTFE own high Mw PTFE that can effectively fiberize and easily disperse into small particle to meet the antidrip purpose.

Intro: GOYENCHEM-PTFE, anti-dropping flame retardant, is provided by GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC GROUP), that work with GY-FR-OP series. When adding into Thermoplastic plastic, due to heat effect, it will generate GOYENCHEM-PTFE microball, which more than 0.18µm, and form cross-link network in the process of pressing and cutting. When burned, this network will contract, then consequently, trap the melted polymer, insulate oxygen, accelerate the carbonization of polymer, and therefore, makes the polymer flame-retarded. GY-PTFE own high Mw PTFE that can effectively fiberize and easily disperse into small particle to meet the antidrip purpose.

Advantages:

  • good anti dropping effect
  • GOYENCHEM-PTFE with high purity and 100% activity
  • great thermal stability
  • good dispersion
  • low dosage
  • high competity with resin
  • can be directly use in resin or plastic
  • simple using and easy storage
  • will not effect the original color
Applications:
  • Engineering plastic including PC, PC/ ABS, ABS, anti dropping
  • Work with GY-FR-OP SERIES, applied on PBT,PET,PA,NYLON flame retard plasic
  • PP?PE?EVA etc. High end flame retard formulation
  • Reach UL94 V-0 with GY-FR-OP SERIES
  • Widely applied on polymers

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Bulk Density
  • Density
  • Particle Mesh Size, 98% pass
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.