MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP21ND-LO Low Outgassing, Room Temperature Curing Two Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Convenient one to one mix ratio
  • Cures at ambient temperatures
  • Passes NASA low outgassing specifications
  • Paste — non-drip application
  • High bond strength
  • Dimensionally stable
Product Description: Master Bond EP21ND-LO is a two component, room temperature curing epoxy system for bonding, sealing and coating featuring outstanding physical properties. EP21NDLO has a convenient one to one mix ratio by weight. It has a paste-like viscosity after mixing. EP21ND-LO can be applied without sagging or dripping even on vertical surfaces. EP21ND-LO produces high strength, durable bonds which hold up well to thermal cycling and resist many chemicals including water, oils, fuels, acids, bases and salts. It is serviceable over the wide temperature range of -60°F to +250°F. It bonds well to a variety of substrates including metals, glass, ceramics, wood, rubber and many plastics. Once cured, EP21ND-LO is an excellent electrical insulator. The standard color of the cured material is gray. Most importantly, EP21ND- LO passes NASA low outgassing specifications as per ASTM E595. To optimize its properties, the best cure schedule for this system is 12-24 hours at room temperature, plus another 2 hours at 150-200°F. This exceptionally versatile system is widely used in the electronic, electrical, computer, metalworking, appliance, chemical, aerospace and OEM industries.

Product Advantages:

  • Convenient mixing, one to one mix ratio by weight
  • Easily applied; adhesive spreads smoothly; non-drip application feature
  • High bonding strength to a wide variety of substrates
  • Excellent dimensional stability
  • Good electrical insulation properties
  • Superior durability, thermal shock and chemical Resistance
  • Passes NASA low outgassing specifications
  • Lower shrinkage upon cure

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Hardness, Shore D
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Compressive Strength
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time, plus 2 hrs at 150-200°F, Optimal cure
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.