MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Inovyn 250SB Polyvinyl Chloride General Purpose - Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Made by suspension polymerization.

APPLICATIONS
Injection :
moldings with complex flow paths
Pressing : mixed with VC-VAc copolymers for gramophone records
Calendering : rigid films and sheets ; used in blend with a suspension resin with a higher K value
Blow molding : alone or mixed with resins with a higher K value : especially injection-blow molding of bottles
All applications : mixed with suspension resins with a higher K value, for easy gelling and increased productivity.

Information provided by SolVin.

SolVin is a predecessor company to Inovyn.

Vendors:
Available Properties
  • Volatile Organic Compounds (VOC) Content, ISO 1269
  • Apparent Bulk Density, ISO 60
  • Particle Size, ISO 1624, >80% greater than value
  • Particle Size, ISO 1624, <2% greater than value
  • Viscosity Test, ISO 1628-2, Reduced viscosity, K value = 50
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Inovyn, SolVin

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.