MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
SABIC LNP™ STAT-KON™ Compound EX07311P Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: LNP STAT-KON EX07311P compound is based on Polyetherimide (PEI) resin containing carbon fiber (15%), glass fiber (25%) and PTFE. Added features of this grade include: LNP Clean Compounding Technology, Electrically Conductive, Dimensional Stability, Wear Resistant.

Features: LNP Clean Compound Technology,High Stiffness,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),Good dimensional stability,Wear resistant,Electrically Conductive

Information provided by SABIC

Vendors:
Available Properties
  • Density, ASTM D792
  • Density, ISO 1183
  • Moisture Absorption, Injection Molding
  • Viscosity, ISO 1133, MVR cc/10 min
  • Linear Mold Shrinkage, Flow, SABIC method
  • Linear Mold Shrinkage, Transverse, SABIC method
  • Tensile Strength at Break, ISO 527, 5 mm/min
  • Tensile Strength at Break, ASTM D638, 5 mm/min
  • Elongation at Break, ISO 527, 5 mm/min
  • Elongation at Break, ASTM D638, 5 mm/min
  • Tensile Modulus, ASTM D638, 5 mm/min
  • Tensile Modulus, ISO 527, 1 mm/min
  • Flexural Strength, ASTM D790, brk, 1.3 mm/min, 50 mm span
  • Flexural Strength, ISO 178, yield, 2 mm/min
  • Flexural Modulus, ASTM D790, 1.3 mm/min, 50 mm span
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Strain at Break, ISO 178, 2 mm/min
  • Izod Impact Notched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180/1A, 80*10*4
  • Coefficient of Friction, Dynamic, ASTM D3702 Modified: Manual
  • K (wear) Factor, ASTM D3702 Modified: Manual, Washer
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Surface Resistance, IEC 60093, ROA
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Af, Flatw 80*10*4 sp=64mm
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Nozzle Temperature
  • Zone 2
  • Zone 3
  • Melt Temperature, Injection Molding
  • Mold Temperature
  • Drying Temperature, Injection Molding
  • Dry Time, Injection Molding
  • Back Pressure
  • Vent Depth
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.