MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Syensqo (Solvay Specialty Polymers) Virantage® VW-10300 P, FP & SFP Polyethersulfone (PESU), Amorphous
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Amorphous, high-temperature sulfone polymer powder, features non-functionalized end groups

Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Three grades are offered: Virantage® VW-10300P, Virantage® VW-10300FP, and Virantage® VW-10300SFP providing three particle sizes to meet formulators' specific needs. Their inherent toughness imparts damage tolerance to thermoset composites. Virantage® PESU polymers also offer superior thermal and hydrolytic stability that deliver best-in-class hot-wet performance.

These amorphous thermoplastics may be used to toughen a variety of advanced thermoset composites used to produce high-performance aerospace components. Virantage® PESU tougheners have been used successfully in a variety of thermosetting resin systems including epoxies, phenolics and BMIs.

All Virantage® PESU polymers are produced at Solvay's state-of-the-art, world-scale facility in Panoli, India under ISO 9001:2000 and ISO 14001:2004 certified quality management systems.

Typical Particle Size ~D90
- VW-10300FP 63.0 µm
- VW-10300P 500 µm
- VW-10300SFP 45.0 µm

Markets/Uses: Composites / Advanced Composites / High-Temperature Tougheners

Applications: Aerospace Applications

Features: Amorphous; Good Thermal Stability; Good Toughness; High Heat Resistance; Hydrolytically Stable; Medium Molecular Weight; Medium-high Viscosity

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Particle Size
  • Viscosity, ASTM D445, Solution Viscosity
  • Glass Transition Temp, Tg, ASTM E1356
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.