MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Carlson C 600ESR Nickel-Chromium-Iron Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: General Description

Carlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excellent resistance to chloride-ion stress corrosion cracking and imparts resistance to corrosion by a number of organic and inorganic compounds. Chromium gives this alloy its resistance to oxidation at temperatures up to 2150°F (1175°C).

C 600 combines high strength with desirable workabi8lity. It has excellent mechanical properties from sub-zero to elevated temperatures.

Applications

  • Chemical Processing – calcium and magnesium chloride production; hydrofluoric acid processes; catalyst support equipment in nitric acid production; ammonia converters; tubing, bends and flanges in vinylchloride production; fluorination reactors; fatty acid vessels; and chlorination equipment.
  • Pulp and Paper – liquid heater tubing for pulp digesters; reactors and piping for disposal of organic wastes; sulfate and soda digester linings
  • Ore Processing – chlorine preheaters for zirconium and titanium production; cans for purification of zirconium salts; titanium dioxide production; reactors for manufacturing aluminum fluoride.
  • Food Processing – vegetable processing equipment
  • Thermal Processing – equipment for heat treating muffles, retorts, baskets and boxes, furnace fixtures and radiant tubing.
  • Power Generation – nuclear reactors components and steam-turbine crossover bellows.

Information provided by Carlson

Key Words: UNS N06600
Vendors:
Available Properties
  • Density
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Poissons Ratio, Calculated
  • Shear Modulus
  • Electrical Resistivity
  • Magnetic Permeability, 200 Oersted
  • Curie Temperature
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Melting Point
  • Solidus
  • Liquidus
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Manganese, Mn
  • Nickel, Ni
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.