MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: Description: IStat-Rite® E-1150 blend is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1150 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite alloys retain uniform static dissipation properties even when injection molded or extruded.

Features:

  • Permanently static dissipative
  • Humidity independent
  • See-through clarity
  • No particulates
  • Ultra-clean: low off-gassing, low ionics, low particulates

Applications:

  • Cleanroom soft walls, windows and doors
  • Vacuum tubing
  • Work surface mats

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength at Break, ASTM D412
  • Elongation at Break, ASTM D412
  • 100% Modulus, ASTM D412
  • 300% Modulus, ASTM D412
  • Tear Strength, ASTM D646
  • Volume Resistivity, ASTM D257
  • Surface Resistivity per Square, ASTM D257
  • Static Decay, FTMS-101C , 12% RH (+5000 V to 50 V)
  • Static Decay, FTMS-101C, 12% RH (-5000 V to -50 V)
  • Drying Temperature, dehumidifying hopper
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lubrizol (former Noveon)

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.