MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Protective Coating PC-Concrete™ Epoxy Concrete Anchoring and Repair System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: PC Concrete™ epoxy gel is an anchoring and concrete repair product. PC Concrete™ is formulated for anchoring threaded rods, bolts, rebar dowels and smooth dowels into concrete, grout filled block, and unreinforced masonry. It has exceptional strength, maximum field reliability, along with a high heat deflection temperature of 134°F.

PC Concrete™ is excellent for filling and repair cracks in concrete, performs better than caulks and hydraulic cement, will not come loose from any cleaned concrete surface, and holds during expansion and contraction of concrete.

PC Concrete™ is a two component (1:1 ratio), 100% solids, high modulus, and structural epoxy gel. It is a solvent free, no odor, high strength, moisture-insensitive epoxy. In addition, PC Concrete™ has a long working time (20 minutes at 75°F.), while providing a bolt down/paint time in as little as 4 hours.

Data provided by the manufacturer.

Key Words: PC Epoxy
Vendors:
Available Properties
  • Water Absorption
  • Storage Temperature
  • Tensile Strength, ASTM D695, 7 Day Cure
  • Elongation at Break, ASTM D638, 7 Day Cure
  • Compressive Yield Strength, ASTM D695, 7 Day Cure
  • Compressive Modulus, ASTM D695, 7 Day Cure
  • Adhesive Bond Strength, ASTM C882, 2 Day Cure
  • Adhesive Bond Strength, ASTM C882, 14 Day Cure
  • Maximum Service Temperature, Air, ASTM D648, Heat Deflection
  • Cure Time
  • Working Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Protective Coating Company

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.