MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Phillips 66 Synterra® ISO Grade 46 Hydraulic Fluid  (discontinued **)
Categories: Fluid; Lubricant

Material Notes: Synterra Hydraulic Fluid is premium quality, synthetic antiwear hydraulic fluid specifically developed for use in industrial and mobile equipment operating in environmentally sensitive areas. It is readily biodegradable for reduced environmental impact in case of leaks or spills. It is particularly recommended for use in hydraulic equipment operating in national parks, ski resorts, wildlife refuges, around lakes and streams, and in other recreational areas. Synterra Hydraulic Fluid is formulated with synthetic polyol ester (POE) base oil and an ashless (zinc-free) antiwear additive package to provide excellent performance over a wide temperature range. It provides excellent wear protection for hydraulic pumps and motors, and protects hydraulic system components against rust and corrosion. It has good oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. This product is nontoxic to the environment and is readily biodegradable. It exceeds all requirements for biodegradability as defined by the EPA 40 CFR Part 792, OECD 301B and USTC PRO/BIO-BP 111-9 test methods. It passes the visual “no sheen” requirements of the U.S. EPA Static Sheen Test. Synterra Hydraulic Fluid meets the performance requirements of all major hydraulic pump manufacturers, and is recommended for use in all types of high-pressure, high-speed hydraulic pumps.

Applications:

  • Mobile and stationary equipment operating in environmentally sensitive areas
  • Boat lifts
  • Chain drives
  • Electrical service bucket trucks (cherry pickers)
  • Farm implements
  • Forestry and logging equipment
  • Marine and offshore equipment
  • Mining equipment
  • Mobile construction equipment
  • Pivots in irrigation systems
  • Ski lifts
Synterra Hydraulic Fluid meets the requirements of the following industry and OEM specifications:
  • Bosch Rexroth AG RE 90 221, Environmentally Acceptable Hydraulic Fluids for Axial Piston Units, Type HEES (approved)
  • Denison Hydraulics HF-0, HF-1, HF-2
  • DIN 51524 Part 2, Antiwear Hydraulic Oils, Type HLP
  • German Steel Industry SEB 181222
  • ISO 11158:1997, Family H (Hydraulic Systems), Type HM
  • U.S. EPA/U.S. Coast Guard Static Sheen Test, Federal Register Vol. 58, No. 41
  • U.S. Steel 127
  • Vickers (Eaton) M-2950-S, I-286-S
Features/Benefits:
  • Nontoxic
  • Readily biodegradable for reduced environmental impact in case of leaks or spills
  • Excellent wear protection for hydraulic pumps and motors
  • Good oxidation resistance and thermal stability
  • Protects against rust and corrosion
  • Excellent storage stability
  • Good foam resistance
  • Excellent low-temperature properties for cold start-ups

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Viscosity Measurement, Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Oxidative Stability, ASTM D2272, RPVOT
  • ASTM Color, ASTM D1500
  • Total Acid Number, ASTM D974, [mg KOH/g]
  • Four Ball Wear, ASTM D4172, Scar Diameter
  • Pour Point
  • Flash Point, COC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.