Application: Greenflex FH 45 is recommended for silage stretch film application to ensure optimum cling properties when used in combination with other cling agent, production of co-extrusion film, lamination film, standard stretch film, stretch hood, barrier film for food packaging, agricultural film.
Film properties are typical of a blown film extruded at 160°C.