Product Description: Bicor HSH is a one-side treated, one-side sealable, coextruded OPP film designed for use in unsupported plain or surface print high-speed horizontal applications. Availability: Latin America, North America and South America Key Features: - Excellent optics
- Excellent hot slip properties for high-speed applications
- Low MST, broad seal range layer
- Non-migratory slip system for consistent COF
Features:- In Lamination Lap Sealable
Applications:- Bakery
- Biscuts/Cookie/Crackers
- Confectionery, Gum
- Confectionery, Sugar
- Crips and Snacks
Uses:Processing Method: Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print UnsupportedInformation provided by ExxonMobil Chemical |