MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
FKuR Kunststoff Bio-Flex® F 1130 Compostable PLA Blend
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any starch or starch derivatives. Bioplastics generally replace conventional materials such as low density polyethylene (LDPE), high density polythene (HDPE) as well as polystyrene (PS) and polypropylene (PP). For packaging applications these materials need to be converted into film which is as thin as possible while maintaining high tensile strength. Depending on the specific application, packaging films have to provide a high barrier against humidity, oxygen and aromas or alternatively provide adequate permeability (“breathability”).

Information Provided by FKuR Kunststoff GmbH

Key Words: Polylactic Acid; biodegradable film
Vendors:
Available Properties
  • Bulk Density, ISO 60
  • Density, ISO 1183
  • Water Vapor Transmission, ISO 15 106-3
  • Oxygen Transmission Rate, ISO 15 105-2, 1 bar
  • Nitrogen Transmission, DIN 53380-2
  • Melt Flow, ISO 1133
  • Film Tensile Strength at Yield, MD, ISO 527-3, BUR 2.3
  • Film Tensile Strength at Yield, TD, ISO 527-3, TD, BUR 2.3
  • Tensile Strength, Yield, ISO 527
  • Film Elongation at Break, MD, ISO 527-3, BUR 2.3
  • Film Elongation at Break, TD, ISO 527-3, BUR 2.3
  • Film Elongation at Yield, MD, ISO 527-3, BUR 2.3
  • Film Elongation at Yield, TD, ISO 527-3, BUR 2.3
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527
  • Tensile Modulus, ISO 527-3, Film TD, BUR 2.3
  • Tensile Modulus, ISO 527-3, Film MD, BUR 2.3
  • Flexural Strength, ISO 178, at 3.5% strain
  • Flexural Modulus, ISO 178
  • Charpy Impact Unnotched, ISO 179-1/1eU
  • Charpy Impact, Notched, ISO 179-1/1eA
  • Elmendorf Tear Strength, MD, ASTM D 1922, BUR 2.3
  • Elmendorf Tear Strength, TD, ASTM D 1922, BUR 2.3
  • Film Tensile Strength at Break, MD, ISO 527-3, BUR 2.3
  • Film Tensile Strength at Break, TD, ISO 527-3, BUR 2.3
  • Melting Point, ISO 3146-C
  • Vicat Softening Point, ISO 306, A
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
FKuR Kunststoff GmbH

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.