Available Properties |
---|
- Specific Gravity, ASTM D792
- Moisture Absorption, ASTM E595, Loss during outgassing
- Outgassing - Total Mass Loss, ASTM E595
- Collected Volatile Condensable Material, ASTM E595
- Tensile Strength, Ultimate, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
- Tensile Strength, Ultimate, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
- Tensile Strength, Yield, ASTM D638, ZX Orientation, Type 1, 0.2 in./min
- Tensile Strength, Yield, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
- Elongation at Break, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
- Elongation at Break, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
- Elongation at Yield, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
- Elongation at Yield, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
- Tensile Modulus, ASTM D638, ZX Orientation, Type 1, 0.2 in./min
- Tensile Modulus, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
- Flexural Strength, ASTM D790, ZX Orientation, Type 1, 0.05 in./min
- Flexural Strength, ASTM D790, XZ Orientation, Type 1, 0.05 in./min
- Flexural Modulus, ASTM D790, ZX Orientation, Type 1, 0.05 in./min
- Flexural Modulus, ASTM D790, XZ Orientation, Type 1, 0.05 in./min
- Flexural Strain at Break, ASTM D790, ZX Orientation, Type 1, 0.05 in./min
- Flexural Strain at Break, ASTM D790, XZ Orientation, Type 1, 0.05 in./min
- Compressive Yield Strength, ASTM D695, ZX Orientation, Method 1, 0.05 in./min
- Compressive Yield Strength, ASTM D695, XZ Orientation, Method 1, 0.05 in./min
- Compressive Strength, ASTM D695, Ultimate, ZX Orientation, Method 1, 0.05 in./min
- Compressive Strength, ASTM D695, Ultimate, XZ Orientation, Method 1, 0.05 in./min
- Compressive Modulus, ASTM D695, ZX Orientation, Method 1, 0.05 in./min
- Compressive Modulus, ASTM D695, XZ Orientation, Method 1, 0.05 in./min
- Izod Impact, Notched, ASTM D256, ZX Orientation, Method A
- Izod Impact, Notched, ASTM D256, XZ Orientation, Method A
- Izod Impact, Unnotched, ASTM D256, ZX Orientation, Method A
- Izod Impact, Unnotched, ASTM D256, XZ Orientation, Method A
- Volume Resistivity, ASTM D257, XY
- Volume Resistivity, ASTM D257, ZX
- Dielectric Constant, ASTM D150-98, XY
- Dielectric Constant, ASTM D150-98, ZX
- Dissipation Factor, ASTM D150-98, ZX
- Dissipation Factor, ASTM D150-98, XY
- CTE, linear, ASTM E831, X
- CTE, linear, ASTM E831, Z
- CTE, linear, ASTM E831, Y
- Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
- Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
- Glass Transition Temp, Tg, ASTM D7426-08
|
| | |