MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond EP4NS-80 One component, Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Low viscosity
  • Not premixed and frozen
  • High glass transition temperature
  • Can be used for underfill and impregnation
Product Description: Master Bond EP4NS-80 is a one component, exceptionally low viscosity epoxy for bonding and sealing. Typically, curing is at 80°C for 2-4 hours, and for full optimization of properties, this should be followed by 110-125°C for 1-2 hours. Since it is not premixed and frozen, it is a true one part system, and has an unlimited working life at room temperature. Storage in a refrigerator is recommended. EP4NS-80 possesses excellent dimensional stability, low CTE and minimal shrinkage upon curing. This epoxy bonds well to a variety of substrates such as metals, composites, ceramics and many plastics. Even though it has very low viscosity, it has good tensile strength as well as an exceptionally high tensile modulus. Its optical properties permit good light transmission from 360 nm to 1500 nm. Its low viscosity allows it to be applied by brushing, spraying or even by spin coating. EP4NS-80 has good chemical resistance to water, oils and fuels, as well as acids and bases. Its color is clear. This epoxy is a reliable electrical and thermal insulator. The service temperature range is -62°C to +232°C (-80°F to +450°F). EP4NS-80 can be considered in optical, aerospace, electronics and specialty OEM applications where a low viscosity epoxy is needed. It is especially useful for laminating, impregnating, and underfill applications. In fiber optics, a typical usage is for sealing fibers into ferrules. This system is also an attractive candidate for sealing and protecting coil windings in harsh environments.

Product Advantages:

  • Single component, no mixing needed
  • Convenient handling and curing schedules
  • User friendly packaging
  • For sealing, impregnation and underfill
  • Excellent optical clarity

Information provided by Master Bond, Inc.

Vendors:
Available Properties
  • Specific Gravity
  • Solids Content
  • Viscosity
  • Hardness, Shore D
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Compressive Strength
  • Adhesive Bond Strength, lap shear, aluminum to aluminum
  • Volume Resistivity
  • Dielectric Constant
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Refractive Index
  • Cure Time, followed by 1-2 hours at 110-125°C
  • Shelf Life, in a refrigerator
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.