MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Wacker Elastosil® R 750/40 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Vulcanizates of ELASTOSIL® R 750/40 silicone rubber possess particularly good resistance to high temperature, oxygen and dry heat.

Application: ELASTOSIL® R 750/40 is optimized for applications at high temperatures and can be used for extrusion and molding applications. Vulcanizates of ELASTOSIL® R 750/40 can withstand temperatures of 300 °C for at least seven days.

Information provided by Wacker Chemie AG.

Vendors:
Available Properties
  • Density, ISO 1183-1 A
  • Hardness, Shore A, using 3% EL AUX STAB H6, curing Agent E
  • Hardness, Shore A, using 3% EL AUX STAB H6, curing Agent C1
  • Hardness, Shore A, DIN 53505 A, curing Agent C1
  • Hardness, Shore A, DIN 53505 A, curing Agent E
  • Hardness, Shore A, using 3% EL AUX STAB H6, curing Agent E, Hot-air aged
  • Hardness, Shore A, using 3% EL AUX STAB H6, curing Agent C1, Hot-air aged
  • Hardness, Shore A, using 3% EL AUX STAB H6, curing Agent C1, Hot-air aged
  • Hardness, Shore A, using 3% EL AUX STAB H6, curing Agent E, Hot-air aged
  • Tensile Strength at Break, using 3% EL AUX STAB H6, curing Agent E
  • Tensile Strength at Break, using 3% EL AUX STAB H6, curing Agent C1
  • Tensile Strength at Break, DIN 53504 S1, curing Agent E
  • Tensile Strength at Break, DIN 53504 S1, curing Agent C1
  • Tensile Strength at Break, using 3% EL AUX STAB H6, curing Agent C1, Hot-air aged
  • Tensile Strength at Break, using 3% EL AUX STAB H6, curing Agent C1, Hot-air aged
  • Tensile Strength at Break, using 3% EL AUX STAB H6, curing Agent E, Hot-air aged
  • Tensile Strength at Break, using 3% EL AUX STAB H6, curing Agent E, Hot-air aged
  • Elongation at Break, using 3% EL AUX STAB H6, curing Agent E
  • Elongation at Break, DIN 53504 S1, curing Agent E
  • Elongation at Break, using 3% EL AUX STAB H6, curing Agent C1
  • Elongation at Break, DIN 53504 S1, curing Agent C1
  • Elongation at Break, using 3% EL AUX STAB H6, curing Agent E, Hot-air aged
  • Elongation at Break, using 3% EL AUX STAB H6, curing Agent C1, Hot-air aged
  • Elongation at Break, using 3% EL AUX STAB H6, curing Agent C1, Hot-air aged
  • Elongation at Break, using 3% EL AUX STAB H6, curing Agent E, Hot-air aged
  • Rebound, DIN 53512, curing Agent C1
  • Rebound, DIN 53512, curing Agent E
  • Tear Strength, ASTM D624 B, curing Agent E
  • Tear Strength, ASTM D624 B, curing Agent C1
  • Compression Set, DIN ISO 815-B, curing Agent C1
  • Compression Set, DIN ISO 815-B, curing Agent E
  • Cure Time, post cured 4h/200°C, E crosslinker
  • Cure Time, post cured 4h/200°C, C1 crosslinker
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.