MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Axiall 5006 Rigid PVC, Extrusion, Natural  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf 5006 Natural is a rigid PVC pellet compound designed for extrusion of interior rigid PVC profiles and various contours where high gloss and ease of processing is required. Georgia Gulf 5006 is widely used for high gloss custom profile, sheet applications. USDA approval allows for use in walk-in coolers and refrigerated trucks. Single or twin screw machines may be used to convert Georgia Gulf 5006. It has been designed with good impact at ambient temperatures. The high flexural and tensile strength make it highly suitable for structural installation. The extrusion flow characteristics are excellent in complicated profiles. It is easily colored using concentrates.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors:
Available Properties
  • Specific Gravity, ASTM D-792
  • Hardness, Rockwell R, ASTM D-785
  • Hardness, Shore D, ASTM D-2240
  • Tensile Strength, Yield, ASTM D-638
  • Tensile Modulus, ASTM D-638
  • Flexural Strength, ASTM D-790
  • Flexural Modulus, ASTM D-790
  • Izod Impact, Notched, ASTM D-256
  • Izod Impact, Notched, ASTM D-256
  • Tensile Impact Strength, ASTM D-1822
  • CTE, linear, ASTM D-696
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D-648
  • Flammability, UL94
  • Melt Temperature
  • USDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Axiall Corporation; formerly Georgia Gulf

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.