MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Total 7835XM Polypropylene, Blow Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade

Material Notes: Random copolymer injection stretch blow molding grade

Clarified - FINA 7835XM offers the ultimate in clarity and gloss.

Impact Strength - FINA 7835XM offers an excellent balance of impact strength and stiffness.

High Purity - FINA 7835XM features minimum taste and odor, an optimum thermal stability for superior color and processability.

FDA - FINA 7835XM complies with all applicable FDA regulations and may be used under those provisions for food contact and packaging.

Recommended Applications - FINA 7835XM is optimized for injection stretch blow molding of containers for drug, cosmetic and toiletry applications requiring exceptional clarity.

Processing - FINA 7835XM resin processes on conventional blow molding equipment with typical melt temperatures of 390-450°F (199-232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors:
Available Properties
  • Water Vapor Permeability, ASTM E96, 90% RH
  • Density, ASTM D1505
  • Oxygen Transmission, ASTM D1434, cc-mm/m²-24hr-atm
  • Linear Mold Shrinkage, ASTM D955
  • Tensile Strength, Ultimate, ASTM D638
  • Elongation at Break, ASTM D638
  • Modulus of Elasticity, ASTM D638
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256A
  • Melting Point, DSC
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Melt Temperature, blow molding
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Total Atofina

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.