MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
SABIC FLEX NORYL™ Resin WCP841 Polyphenylene Ether + TPE (PPE+TPE) (Americas)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyphenylene Ether/PPO

Material Notes: FLEX NORYL™ WCP841 resin is flexible, non-reinforced injection moldable blend of polyphenylene ether (PPE) + thermoplastic elastomer (TPE). This material contains non-halogenated flame retardant and carries a UL94 flame rating of V0 at 6mm. FLEX NORYL WCP841 resin is intended for evaluation in over-molding applications such as plugs, strain reliefs, and connectors. It has a Shore A Hardness reading of 84 and exhibits low specific gravity, very low water absorption, and dimensional stability.

Features: Flexible,Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Thin Wall,Non-Halogenated,Non-Chlorinated,Non-Brominated,Good Processability,Ductile

Information provided by SABIC

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption, Injection Molding
  • Linear Mold Shrinkage, Flow, ASTM D955, 24hrs
  • Linear Mold Shrinkage, Transverse, ASTM D955, 24hrs
  • Melt Flow, ASTM D1238
  • Melt Flow, ASTM D1238
  • Hardness, Shore A, ASTM D2240, 30s reading
  • Tensile Strength at Break, ASTM D638, 50 mm/min
  • Tensile Strength at Break, ISO 527, 50 mm/min
  • Elongation at Break, ASTM D638, 50 mm/min
  • Elongation at Break, ISO 527, 50 mm/min
  • Flexural Modulus, ASTM D790, 12.5 mm/min, 100 mm span
  • Flexural Modulus, ISO 178, 12.5 mm/min
  • Volume Resistivity, ASTM D257
  • Comparative Tracking Index, UL 746A
  • Comparative Tracking Index, IEC 60112
  • Brittleness Temperature, ASTM D746
  • Flammability, UL94, UL 94
  • Flammability, UL94, UL 94
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Nozzle Temperature
  • Zone 2
  • Zone 3
  • Melt Temperature, Injection Molding
  • Mold Temperature
  • Drying Temperature, Injection Molding
  • Dry Time, Injection Molding
  • Dry Time, Cumulative; Injection Molding
  • Back Pressure
  • Shot Size
  • Vent Depth
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.