MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.
Lucas-Milhaupt SIL-FOS® 15 Copper-Copper Brazing (Silvaloy® 15 Excel)
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes: Sil-Fos 15 is the preferred alloy for general copper-copper brazing; the phosphorous in the Sil-Fos family serves as a fluxing agent, no flux is recommended. Sil-Fos 15 is the best alloy to use when joining metals where close fit-ups cannot be maintained and is well suited for use in refrigeration applications. Applications: HVAC/R Refrigerant systems, air conditioning coils, evaporator coils. Sil-Fos 15 and was developed primarily for use on copper, but its use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditioning apparatus, electrical conductors, copper and brass pipe fittings, and other copper and brass equipment. Brazing characteristics: Sil-Fos 15 is a copper rich, filler metal that is self-fluxing on copper by virtue of its phosphorus content. The self-fluxing property of this filler metals is effective on copper only. With copper-base alloys, such as brass or bronze, the joints should be fluxed with Handy Flux ®. Sil-Fos 15 should not be used on nickel-base and iron-base alloys, as the phosphorus reacts with the nickel or iron to form brittle compounds at the interface of the joints. Sil-Fos 15 has a strong tendency to liquate (i.e. to separate into low and high melting constituents) if heated slowly through its melting range, as normally occurs in furnace brazing. The results in leaving a “skull” of unmelted alloy behind may objectionable from the standpoint of appearance. In furnace brazing it is preferable to pre-place the alloys inside the joint where the skull is not visible. The properties of a brazed joint are dependent upon numerous factors including base metal properties, joint design, metallurgical interaction between the base metal and the filler metal. Normally the corrosion resistance of Sil-Fos 15 is of the same order as copper, but under certain conditions it may corrode more rapidly. Sil-Fos 15 should not be used where the joints are exposed to sulfur compounds, especially in gasses or oils at temperatures above normal room temperature. Exposure to pressured steam can also result in accelerated corrosion.

Available forms: Wire, strip, engineered preforms, specialty preforms, powder and paste.

Information provided by Lucas-Milhaupt.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Electrical Resistivity, 9.9% IACS
  • Melting Point
  • Solidus
  • Liquidus
  • Processing Temperature, Brazing Range
  • Copper, Cu
  • Other, total
  • Phosphorus, P
  • Silver, Ag
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

solder replacement adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.