Temper: Mill-hardened Temper, TM - SHM Fabrication Properties: Excellent Suitability – Capacity for Being Hot Formed; Good Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Capacity for Being Cold Worked; Fair Suitability – Spot Weld, Seam Weld, Butt Weld Typical uses: Electrical Connectors – Automotive; Connector Components |