MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
ITW Plexus® MA830 Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Plexus® MA830 is a two-part methacrylate adhesive designed for structural bonding of metals without primers. In addition, MA830 does a superb job of bonding thermoplastic and composite assemblies with little or no surface preparation. Combined at a 10:1 ratio, MA830 has a working time of 4 to 6 minutes and achieves approximately 75% of ultimate strength in 15 to 25 minutes at 74°F (23°C). This product provides a unique combination of high strength, excellent fatigue endurance, outstanding impact resistance, and superior toughness. Plexus MA830 is supplied in a ready-to-use to be dispensed as a non-sagging gel.

Excellentl resistance to: ? Hydrocarbons ? Acids and Bases (pH 3-10) ? Salt Solutions. Susceptible to: ? Polar Solvents ? Strong Acids and Bases. Recommended for: ? ABS ? Acrylics ? Aluminum ? FRP ? Gel coats ? PVC ? Polyesters (including DCPD modified) ? Steel (Exterior applications require the use of coatings or primers that inhibit oxidation of the steel.) ? Styrenics ? Urethanes (general) ? Vinyl Esters. Adhesive color: off white, uncured-room temperature. Activator color: gray or gray GB, uncured-room temperature.

Information provided by ITW Performance Polymers.

Vendors:
Available Properties
  • Density, adhesive. Uncured.
  • Density, Cured
  • Density, Activator. Uncured.
  • Density, Activator. Uncured.
  • Volatile Organic Compounds (VOC) Content, During cure
  • Viscosity, Activator
  • Viscosity, Adhesive
  • Hardness, Shore D, ASTM D2240, cured-room temperature.
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Adhesive Bond Strength, ASTM D1002, Lap Shear Cohesive Strength
  • Tensile Impact, ASTM D950
  • Tensile Impact, ASTM D950
  • Peel Strength, ASTM D1876
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flash Point
  • Working Life
  • Shelf Life, Activator (B side)
  • Shelf Life, Cartridges
  • Shelf Life, Adhesive (A side)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.