MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Morgan Advanced Ceramics GBC-99.5% Alumina 723U Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: High purity alumina ceramic with excellent mechanical, electrical, thermal, and chemical properties.

Prime Features:

  • Excellent abrasion and temperature resistance
  • High mechanical strength
  • Exceptional purity
  • Chemical and corrosion resistance
  • Excellent dielectric properties
  • Dense, non porous and vacuum tight
Typical Applications:
  • Bearings
  • Wear nozzles
  • Medical implants
  • Pump seals
  • Electronic insulators
  • Bushings
  • Semiconductor
  • Wear resistance components
  • General industrial duties requiring superior mechanical, electrical, and thermal properties
Production Capabilities:
  • High volume production
  • Tight tolerance pressed alumina parts
  • Multi-cavity tooling
  • Complex geometries and multi-level configurations
  • Sub-miniature designs
  • Precise material and batch control
  • Design consultation

Information provided by Morgan Advanced Materials

Key Words: 723U
Vendors:
Available Properties
  • Bulk Density
  • Open Porosity, fully dense, % nominal, apparent
  • Hardness, Mohs
  • Tensile Strength
  • Flexural Strength
  • Compressive Strength
  • Volume Resistivity, at RT
  • Dielectric Constant, at RT
  • Dielectric Strength
  • Dissipation Factor, at RT
  • CTE, linear
  • Thermal Conductivity, at RT
  • Al2O3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.