Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America
Features: Abrasion Resistant; Brominated; Filled; Flame Retardant; Good Colorability; High Flow; Medium Density; High Hardness; Light Stabilized; Lubricated; High Flow; Slip; Sunlight Resistant; UV Resistant
Uses: Flooring; Rubber Replacement
RoHS Compliance: RoHS Compliant
Form: Pellets
Processing Method: Injection Molding
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticThermoplastic Elastomer