MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SABIC NORYLâ„¢ Resin PKN4752 Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL PKN4752 resin is a non-reinforced, translucent, high heat blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This extrudable and injection moldable grade exhibits high heat resistance, dimensional stability, and appears translucent with a yellow tint in the natural color. NORYL PKN4752 resin is an excellent candidate for high performance packaging in food, electronics, and healthcare. *See NORYL PKN4752F resin for FDA food compliant version.

Features: Hydrolytic Stability,Low Creep Sensitivity,High Heat Resistance,Translucent,Low Warpage

Information provided by SABIC

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption, Sheet Extrusion
  • Linear Mold Shrinkage, Flow, SABIC method
  • Tensile Strength at Break, ASTM D638, 50 mm/min
  • Tensile Strength, Yield, ASTM D638, 50 mm/min
  • Elongation at Break, ASTM D638, 50 mm/min
  • Elongation at Yield, ASTM D638, 50 mm/min
  • Tensile Modulus, ASTM D638, 50 mm/min
  • Flexural Strength, ASTM D790, yld, 2.6 mm/min, 100 mm span
  • Flexural Strength, ASTM D790, yld, 1.3 mm/min, 50 mm span
  • Flexural Modulus, ASTM D790, 2.6 mm/min, 100 mm span
  • Flexural Modulus, ASTM D790, 1.3 mm/min, 50 mm span
  • Izod Impact Notched, ASTM D256
  • Dart Drop, Total Energy, ASTM D3763
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, unannealed
  • Vicat Softening Point, ASTM D1525, Rate B/50
  • Zone 1, Sheet Extrusion
  • Zone 2, Sheet Extrusion
  • Zone 3, Sheet Extrusion
  • Zone 4, Sheet Extrusion
  • Adapter Temperature, Sheet Extrusion
  • Die Temperature, Sheet Extrusion
  • Melt Temperature, Sheet Extrusion
  • Roll Temperature, Roll Stack Temp - Bottom
  • Roll Temperature, Roll Stack Temp - Middle
  • Roll Temperature, Roll Stack Temp - Top
  • Drying Temperature, Sheet Extrusion
  • Dry Time, Sheet Extrusion
  • Dry Time, Cumulative; Sheet Extrusion
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saudi Basic Industries Corporation; SABIC Innovative Plastics (GE Plastics)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.