MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
UBE Upilex® 50VT Polyimide Film
Categories: Polymer; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: UPILEX®-VT and UPILEX®-NVT are heat bonding polyimide films having heat fusing layers on both side of the film, created by the polyimide resin equivalent of UPILEX®-S. High quality flexible circuits without an adhesive layer are obtained, by heating and pressing UPILEX®-VT or UPILEX®-NVT with metal (Cu, SUS, Al) foil. In addition, they are also available for bonding films comprised of metal, ceramic and other materials. Flexible circuits without adhesive are produced. This offers high tensile strength and tear strength. Offering the same low water absorption, low dimensional change and high heat resistance as UPILEX®-S, with the addition of laminate workability in the heat press.

Information provided by UBE Industries, LTD

Vendors:
Available Properties
  • Density, ASTM D1505-03
  • Water Absorption, ASTM D570
  • Tensile Strength, ASTM D882
  • Elongation at Break, ASTM D882
  • Tensile Modulus, ASTM D882
  • Tear Strength, IPC-TM-650 2.4.17.1
  • Volume Resistivity, ASTM D257, DC 100V
  • Surface Resistance, ASTM D257, DC 100V
  • Dielectric Constant, Triplate-Line Resonator
  • Dielectric Constant, Triplate-Line Resonator
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, Triplate-Line Resonator
  • Dissipation Factor, Triplate-Line Resonator
  • CTE, linear, Fine linear dilatometer
  • Decomposition Temperature, TG-DTA. In air. @ 5% wieght loss
  • Flammability, UL94
  • Shrinkage, JIS C2318, heat
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.