MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
AGC Fluon® EA-2000 Perfluoro Adhesive
Categories: Polymer; Adhesive

Material Notes: Introduction: Fluon® PFA EA-2000, is an Perfluoro resin which has been functionalized to include an adhesive group within the polymer backbone. The perfluoro backbone gives the material excellent electrical characteristics, and heat and chemical resistance, while the adhesive functionality facilitates adhesion to other materials in a one-step process, without the need for surface treatment or a separate adhesive layer. Example materials include glass cloth, polyimide, or various metals. This grade is semi-commercialized and may be available upon request. This material is supplied as pellets and packaged in 25kg plastic bags.

Features of EA-2000:

  • Heat resistance to 260C and superior chemical resistance, equivalent to conventional PFA materials
  • Adhesion to other polymers and metals without the use of surface treatment or a separate adhesive layer via a traditional melt-processable method.
  • Excellent non-stick properties, low frictional properties, and water and oil repellency (high contact angle)
  • Low dielectric constant (2.1) and low dissipation factor (0.001)
Assumed Applications of EA-2000:
  • Printed circuit boards (rigid or flexible)
  • Heat-resistant insulating tape
  • Heat-resistant laminated tubing
  • Interposers
  • Steel plate laminates

Information provided by AGC Chemicals Americas Inc.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Melt Flow, ASTM D3307
  • Hardness, Shore D
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D368
  • Flexural Modulus, ASTM D790
  • Flex Crack Resistance, ASTM D2176, Cycles per MIT Folding Endurance
  • Izod Impact, Notched, ASTM D256
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dissipation Factor, ASTM D150
  • Specific Heat Capacity
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Asahi Glass Company, AGC Fluorocompounds

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.