MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
CHT Group EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea
Categories: Polymer; Thermoset

Material Notes: RAP-1567 SP-HX is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generation polyurea displays fast cure times and excellent adhesion characteristics. RAP-1567 SP-HX is designed to be quick gelling (30 minutes) in order to optimize leveling and wetting properties. RAP-1567 SP-HX can be spray applied at temperatures ranging from 20ºF to 120ºF. This 100% polyurea elastomer displays excellent chemical resistance, water insensitivity and UV resistance (in any color) at a wide range of temperatures. RAP-1567 SP-HX will provide a smooth glossy finish when fully cured. RAP-1567 SP-HX emits virtually no odors and can be applied indoors without any VOC’s. RAP-1567 SP-HX meet USDA and FDA specifications. RAP-1567 SP-HX can be rolled, brushed, or spray applied thru airless or plural equipment.

Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors:
Available Properties
  • Viscosity, A Side
  • Viscosity, B Side
  • Hardness, Shore D, ASTM 2240
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • Adhesive Bond Strength, ASTM D4541 Elcometer, Wood (no primer), Delamination
  • Adhesive Bond Strength, ASTM D4541 Elcometer, Concrete (primer), Concrete Failure
  • Adhesive Bond Strength, ASTM D4541 Elcometer, Concrete (epoxy), Concrete Failure
  • Adhesive Bond Strength, ASTM D4541 Elcometer, Concrete (no primer), Concrete Failure
  • Adhesive Bond Strength, ASTM D4541 Elcometer, Steel (no primer), Substrate Failure
  • Adhesive Bond Strength, ASTM D4541 Elcometer, Steel (epoxy primer), Primer Failure
  • Tear Strength, ASTM D412
  • Taber Abrasion, mg/1000 Cycles, ASTM D4060, CS17 Wheel, 1kg
  • Flash Point, ASTM Pensky-Martin
  • Tack-Free Time
  • Pot Life
  • USDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.