Applications: Tires. KIBIPOL® HBR is a high-cis butadiene rubber using neodymium (Nd) as the catalyst. It is colorless and odorless. Compared to NiBR or CoBR , NdBR offers better performance for abrasion resistance, rebound ability and strength. KIBIPOL® HBR also delivers the lowest water content in the world, creating a transparent appearance. Information provided by Chi Mei Corporation |