MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.

Information provided by 3M

Vendors:
Available Properties
  • Viscosity, Accelerator
  • Viscosity, Base
  • Hardness, Shore D
  • Shear Strength, Overlap, Isopropyl Alcohol Wipe surface prep, Neoprene/Steel
  • Shear Strength, Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Neoprene/Steel
  • Shear Strength, Overlap, Isopropyl Alcohol Wipe surface prep, Polystyrene
  • Shear Strength, Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polycarbonate
  • Shear Strength, Overlap, Isopropyl Alcohol Wipe surface prep, FRP
  • Shear Strength, Overlap, Isopropyl Alcohol Wipe surface prep, Polycarbonate
  • Shear Strength, Overlap, Isopropyl Alcohol Wipe surface prep, Polyacrylic
  • Shear Strength, Overlap, Isopropyl Alcohol Wipe surface prep, ABS PVC
  • Shear Strength, Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polyacrylic
  • Shear Strength, Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polystyrene
  • Shear Strength, Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, ABS PVC
  • Shear Strength, Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol Wipe surface prep, FRP
  • Shear Strength, Overlap, Isopropyl Alcohol Wipe surface prep, Phenolic
  • Shear Strength, Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Phenolic
  • Shear Strength, Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, SBR/Steel
  • Shear Strength, Overlap, Isopropyl Alcohol Wipe surface prep, SBR/Steel
  • Shear Strength, Overlap, Stainless Steel MEK/abrade/MEK
  • Shear Strength, Overlap, CRS MEK/abrade/MEK
  • Shear Strength, Overlap, Aluminum MEK/abrade/MEK
  • Shear Strength, Overlap, Brass MEK/abrade/MEK
  • Shear Strength, Overlap, Galvanized Steel Hot dipped
  • Shear Strength, Overlap, Galvanized Steel Electrodeposited
  • Shear Strength, Overlap, Antifreeze/H2O (50/50) immersion, 82°C for 30 days
  • Shear Strength, Overlap, Methyl Ethyl Ketone immersion, RT for 30 days
  • Shear Strength, Overlap, Aluminum Oakite degrease
  • Shear Strength, Overlap, Water Vapor, 49°C at 100% RH for 30 days
  • Shear Strength, Overlap, Water Vapor, 93°C at 100% RH for 14 days
  • Shear Strength, Overlap, Skydrol LD-4 immersion, 66°C for 30 days
  • Shear Strength, Overlap, Distilled Water immersion for 30 days
  • Shear Strength, Overlap, Aluminum Etched
  • Shear Strength, Overlap, Isopropyl Alcohol immersion, RT for 30 days
  • Shear Strength, Overlap, RT at 50% RH for 30 days
  • Shear Strength, Overlap, Copper MEK/abrade/MEK
  • Shear Strength, Aluminum Overlap
  • Shear Strength, Aluminum Overlap
  • Shear Strength, Aluminum Overlap
  • Shear Strength, Aluminum Overlap
  • Shear Strength, Aluminum Overlap
  • Shear Strength, Aluminum Overlap
  • Shear Strength, Aluminum Overlap
  • Peel Strength, CRS, T-Peel, 17-20 mil bondline, MEK/abrade/MEK
  • Peel Strength, CRS, T-Peel, 17-20 mil bondline, Oakite degreased
  • Peel Strength, Aluminum Etched, T-Peel, 5-8 mil bondline
  • Peel Strength, Aluminum Etched, T-Peel, 17-20 mil bondline
  • Peel Strength, Aluminum, T-Peel
  • Peel Strength, Aluminum, Bell Peel
  • Peel Strength, Aluminum, T-Peel
  • Peel Strength, Aluminum, Bell Peel
  • Peel Strength, Aluminum, T-Peel
  • Peel Strength, Aluminum, Bell Peel
  • Volume Resistivity, ASTM D257
  • Dielectric Strength, ASTM D149
  • CTE, linear, Below Tg
  • CTE, linear, Above Tg
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.