MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Sika Level-02 EZ Primer Acrylic Primer
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Special Acrylic Primer for use on sound, smooth and non-porous substrates in interior areas. Applied prior to the use of Sika® Level products on epoxy, ceramic tiles, old vinyl, linoleum and rubber coverings.

Where to Use:

  • Many tight substrates like- terrazzo, ceramic tiles, natural stone
  • Old substrates with water-resistant adhesive residues
  • Fully-bonded old elastic coverings
  • Old sealed/coated substrates
  • Epoxy moisture barrier
  • Metal
  • Wood Flooring
  • LVT, PVT.
Advantages:
  • Provides optimum adhesion
  • Ready-to-use, no dilution required
  • Quick dry time
  • Low VOC
  • Solvent free
  • Suitable for application on subfloor radiant system
  • Low consumption of material

Information provided by Sika Corporation.

Vendors:
Available Properties
  • Density
  • Volatile Organic Compounds (VOC) Content, EPA method 24
  • Adhesive Bond Strength, ASTM C882, substrate failure
  • Dry Time
  • Shelf Life, in original unopened cartridge
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.