MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Geon® Performance Solutions 87263 Vinyl Compound - Rigid (RPVC)  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes:

Description/Features:

  • Exterior-Weatherable Natural Base
  • UL 94 V0

Applications:

  • Custom Profiles

Processing Method:

  • Extrusion-Single Screw
PolyOne First Choice

Disclaimer: NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of unpigmented compounds or so-called natural compounds generally is inferior to pigmented compounds. Unpigmented weatherable compounds may also contain non-pigment ingredients which can interact unpredictably with pigments to produce unexpected weathering results. Therefore, in applications where processors or customers would like to use an unpigmented compound, or add their own pigment package, it is the customer’s responsibility to determine whether or not the weathering performance after pigmenting is acceptable in their specific end-use application.
Note: The Cell Classification was determined using the notched Izod test with injection molded samples.

Information provided by PolyOne Corporation.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Hardness, Shore D, ASTM D2240, 15 sec
  • Tensile Strength, Yield, ASTM D638, Type 1 - Rigids, 0.2 in/min
  • Tensile Modulus, ASTM D638, Type 1 - Rigids, 0.2 in/min
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256, Method A, With Grain - Comp. Molded
  • Izod Impact, Notched, ASTM D256, Method A, Against Grain - Comp. Molded
  • Izod Impact, Notched, ASTM D256, Method A, Injection Molded
  • Dart Drop Total Energy, ASTM D4226, Procedure A, 0.125 in Conical Dart, 73°F (23°C)
  • Dart Drop Total Energy, ASTM D4226, Procedure B, 0.125 in Conical Dart, 73°F (23°C)
  • CTE, linear, ASTM D696
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed, 0.125 in bars
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.