| LF2554 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for slot cast extrusion which offers outstanding toughness, extrudability and draw down ability. Applications: Stretch film, high quality packaging film, cast film, diaper film, multilayer film. Advantages: High clarity, high tensile strength, outstanding drawdown capability, good balance of stiffness and puncture resistance. Information provided by Titan Chemicals |