Features: Low Temperature Flexibility, Excellent Abrasion, Fungal, and Chemical Resistance, and Hydrolytic Stability. Adhesives can be applied from solution or extruded as a melt coating. The resin is lightly dusted with calcium stearate and contains UV stabilizer. Uses: Various adhesive and fabric coating, magnetic media binder and cast films for lamination Available in Americas, Europe, Middle East, Africa, India and Asia Information provided by Noveon, Inc. |