MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
ExxonMobil Metallyte™ 18MM488 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A metalized biaxially oriented polypropylene film, metalized on one side. MM488 is typically used in laminates as the inner web for VFFS and HFFS applications. Due to its slip controlled broad seal range surface, film offers excellent performance on all types of VFFS packaging machines. When laminated with standard coex, it can be lap sealed.

Availability: Africa & Middle East, Asia Pacific and Europe

Key Features:

  • Excellent adhesion of aluminum to film
  • Very good moisture barrier and light barrier
  • Slip controlled sealing layer
  • Good oxygen barrier
  • Very good hot tack
  • Broad seal range for good performance on VFFS and HFFS machines
  • Easy to convert
  • Brilliant metal appearance
Features:
  • Flavor & Aroma Barrier
  • Gas Barrier
  • In Lamination Lap Sealable
  • Light Barrier
  • Moisture Barrier
  • Oxygen Barrier
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Box Overwrap
  • Confectionery, Chocolate
  • Confectionery, Gum
  • Confectionery, Sugar
  • Crisps and Snacks
  • Dry Foods and Beverage Powders
  • Frozen Food
  • Ice Cream
  • Pet Food
Uses:
  • Box Overwrap Flexible Packaging
  • HFFS Flexible Packaging
  • Pre-made Bags – Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print Unsupported

Information provided by ExxonMobil

Vendors:
Available Properties
  • Water Vapor Transmission, ExxonMobil Method, 90% RH
  • Oxygen Transmission Rate, ExxonMobil Method, 0% RH
  • Thickness, ExxonMobil Method
  • Coating Weight, ExxonMobil Method
  • Film Elongation at Break, MD, ExxonMobil Method, 7.9 in/min, 4.9 in Jaw Separation
  • Film Elongation at Break, TD, ExxonMobil Method, 7.9 in/min, 4.9 in Jaw Separation
  • Modulus of Elasticity, ExxonMobil Method, MD
  • Modulus of Elasticity, ExxonMobil Method, TD
  • Coefficient of Friction, ExxonMobil Method, Unmetallized Size
  • Seal Strength, ExxonMobil Method, Otto Brugger, 0.2 sec
  • Film Tensile Strength at Break, MD, ExxonMobil Method, 7.9 in/min, 4.9 in Jaw Separation
  • Film Tensile Strength at Break, TD, ExxonMobil Method, 7.9 in/min, 4.9 in Jaw Separation
  • Shrinkage, MD, ExxonMobil Method
  • Shrinkage, TD, ExxonMobil Method
  • Optical Density, ExxonMobil Method
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.