SCG PP P704JM is a homopolymer polypropylene resin that is well-suited to healthcare and pharmaceutical products. P704JM has good process ability, high clarity and is compliant to FDA and USP requirements.P704JM can be injection molded and sterilized by ethylene oxide. Applications: Syringe barrel, Cylindrical test tubes, Contact Lens Mold Shell, Applications required high transparency. Features: Easy processing. High transparency. High stiffness. Information provided by SCG. |