MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
TIMET TIMETAL® 17 Titanium Alloy (Ti-5Al-2Sn-4Mo-2Zr-6Mo); STA
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: High strength, deep hardenable forging near-beta alloy primarily for jet engines. Allows heat treatment to a variety of strength levels in sections up to 6 inches. Offers good ductility and toughness, as well as good low cycle and high cycle fatigue properties.

Typical heat treatment: Solution treat 1475°F for 4 hr and water quench. Age 1175°F for 8 hr and air cool.

Data provided by TIMET.

Key Words: UNS R52252
Vendors:
Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Reduction of Area
  • Creep Strength, 0.2% creep
  • Creep Strength, 0.2% creep
  • Creep Strength, 0.2% creep
  • Creep Strength, 0.2% creep
  • Creep Strength, 0.2% creep
  • Creep Strength, 0.2% creep
  • Rupture Strength
  • Rupture Strength
  • Rupture Strength
  • Rupture Strength
  • Rupture Strength
  • Rupture Strength
  • Rupture Strength
  • Modulus of Elasticity
  • Notched Tensile Strength
  • Notched Tensile Strength
  • Notched Tensile Strength
  • Notched Tensile Strength
  • Notched Tensile Strength
  • Fatigue Strength, Maximum Stress (Load Control A = 0.95)
  • Fatigue Strength, Maximum Stress (Load Control A = 0.95)
  • Fatigue Strength, Maximum Stress (Load Control A = 0.95)
  • Fatigue Strength, Maximum Stress (Load Control A = 0.95)
  • Fatigue Strength, Maximum Stress (Load Control A = 0.95)
  • Fatigue Strength, Maximum Stress (Load Control A = 0.95)
  • Fatigue Strength, Maximum Stress (Load Control A = 0.95)
  • Fracture Toughness, Yield Strength = 1158 MPa (168 ksi)
  • Fracture Toughness, Yield Strength = 1054 MPa (153 ksi)
  • Fracture Toughness, Yield Strength = 1110 MPa (161 ksi)
  • Beta Transus
  • Solution Temperature
  • Aging Temperature
  • Aluminum, Al
  • Chromium, Cr
  • Molybdenum, Mo
  • Other, each
  • Other, total
  • Tin, Sn
  • Titanium, Ti, Calculated as remainder
  • Zirconium, Zr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.