MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Eastman EEH Solvent
Categories: Fluid; Solvent

Material Notes: CAS No. 1559-35-9

Product Description: Eastman™ EEH Solvent (Ethylene Glycol 2-Ethylhexyl Ether) is primarily used in performance specialty coatings applications. It offers an excellent balance of performance properties when used as a coalescent in architectural and industrial maintenance coatings. Eastman™ EEH Solvent has low water miscibility, low surface tension, good hydrolytic stability, and high electrical resistance. In electrodeposition primers, Eastman™ EEH Solvent reduces volatilization from dip tanks and provides good flow and leveling of the coating in the baking oven. It is not a HAP or listed on SARA 313.

Application/Uses:

  • Coatings - Architectural
  • Coatings - Automotive OEM
  • Coatings - Automotive Refinish
  • Coatings - Can and Coil
  • Coatings - Consumer Electronics
  • Coatings - Floor Polishes
  • Coatings - General Industrial
  • Coatings - Industrial Maintenance and Marine
  • Coatings - Industrial Wood
  • Coatings - Transportation
Key Attributes:
  • Efficient coalescent
  • Low surface tension
  • Low water solubility
  • LVP-VOC
  • Non-HAP
  • Non-SARA
  • REACH compliant
  • Readily biodegradable
  • Slow evaporation rate

Information provided by Eastman

Vendors:
Available Properties
  • Density
  • Viscosity, Liquid
  • Vapor Pressure
  • Vapor Pressure
  • Total Acid Number
  • CTE, linear
  • Melting Point, Freezing Point
  • Boiling Point, @ 760 mm Hg, Initial
  • Boiling Point, @ 760 mm Hg, Dry Point
  • Flash Point, Setaflash Closed Cup
  • Refractive Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Eastman Chemical Company

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.