Properties: Kanatol-8080 is transparent liquid with stability and is soluble in most organics solvent. Kanatol-8080 is used in a lot of European countries in application where human body is directly in contact with material like toys, nappy, medical material, artificial leather, water pipe. Kanatol-8080 is not limited as carcinogen DOP. You can add your products as NON CARCINOGEN PRODUCT. It has different structure than phthalic based plasticizers. As a result of this migration is lower. The materials, which are made with K-8080, are more resistant to most of hydrocarbons. It has lower flexibility because of its structure and this decreases fragility. It can lubricate itself because of structural characteristics. Preparing plastisol with K-8080 consumes shorter time and less energy. K-8080 can be replaced with DINP/DIDP because of lower volatile losses. Preferable plasticizer for producing cable with excellent electrical specialties. Application: KANATOL-8080 is a primary plasticizes for soft PVC products and is recommended to be used in high –temperature cable and wire. KANATOL-8080 used in vinyl gloves, wall covering, vinyl flooring, carpet & novelties and synthetic rubber. Chemical Name: Di-(2-ethylhexyl) 1,4 benzene di carboxylate Molecular Formula: C 24 H38 O 4 Molecular Structure: C6 H4 -1,4-[CO 2 CH2 CH(C2 H 5 )(CH2 ) CH3 ] 2 CAS Number: 6422-86-2 EINECS NO: 229-176-9 Information provided by KLJ Group |